Tensile Testing Machines

Back to Index

Stress-Strain Behavior of Polymers

One of the most important characteristics of polymers is their inherent toughness and resistance to fracture (crack propagation). It is not coincidence that the name plastic, which describes any kind of polymeric material, is similar to the word plasticity which is the propensity of a solid to undergo permanent deformation under stress.

The mechanical properties of plastic materials depend on both the strain (rate) and temperature. At low strain, the deformation of most solids is elastic, that is, the deformation is homogenous and after removal of the deforming load the plastic returns to its original size and shape. In this regime, the stress (σ) is proportional to the strain (ε):

Stress = Constant x Strain

or

σ = E ε

where E is the tensile (or Young's) modulus of the plastic which is a measure of the stiffness of the material. This relationship is known has Hooke's law. It means, when a plastic specimen is pulled at a (constant) strain rate the applied stress (or load) is directly proportional to the observed strain (or elongation). The maximum stress up to which the stress and strain remain proportional is called the proportional limit. If a plastic material is loaded beyond its elastic limit, it does not return to its original shape and size, i.e. a permanent deformation occurs. With increasing load a point is eventually reached at which the material starts yielding. This point is known as the yield point. A further increase in strain occurs without an increase in stress.

The stress-strain behavior of a polymer greatly depends on the temperature. At very low temperature well below the glass transition temperature, brittle failure is observed as a break at low strain rate at the stress maximum. If the temperature is increased, a polymeric material changes from brittle (crazing) to ductile (yielding) behavior in deformation and fracture. This temperature is called the brittle-ductile transition temperature (Tβ).1

Stress-Strain Behavior of Polymers

CROW logo

A ductile material shows a characteristic yield point followed by a drop in strength and break at lower stress but much higher strain. At this point, the material starts to undergo plastic deformation. Materials with high plasticity show strong necking and in some cases cold drawing. Beyond the yield point, the cross section in the necking region will steadily reduce until the material breaks abruptly. For some polymers, strong stretching with a stress minimum and break at a much higher stress is observed. This phenomenon is known as "strain hardening" and "stress induced crystallization". It is caused by orientation and allignment of polymer chains in the direction of the load which increases the strength and stiffness of the plastic in stretch direction and explains the observed increase in (true) stress. The opposite of strain hardening is strain softening.  Amorphous polymers, when physically aged, exhibit soemtimes true strain softening.3 In that case, the deformation process progressively removes the effect of aging which leads to a decrease in stress when the specimen is pulled at a constant strain rate. Miehe et al. postulated that the true strain softening is the result of localized shear band formation.4

When the temperature exceeds the glass transition temperature, the plastic material abruptly changes its mechanical behavior. In this region, the ultimate extension can be very high at rather low loads. In some cases, it can exceed several hundred percent before failure occurs. The behavior before break will depend on the crosslink and entanglement density; materials that are lightly crosslinked will undergo large elastic deformation prior break, whereas uncrosslinked polymers will show viscoelastic behavior.

References and Notes
  1. The brittle-ductile transition temperature, Tb, is not always identical with the glass transition temperature, Tg. For example, for very tough plastics like polycarbonate and polysulfone, the ratio Tb / Tg ≈ 0.38, whereas for polyphenyl methacrylate Tb and Tg coincide, Tb / Tg ≈ 1.0.2

  2. Souheng Wu, J. of Appl. Poly. Sci., Vol 46, pages 619-624 (1992)

  3. Strain hardening is sometimes erroneously called "strain softening" when the shear or tensile resistance decreases with increasing strain. The observed drop in stress beyond the yield point is caused by a reduction of the cross section area (necking). The true stress, however, which is the load divided by the actual cross-sectional area, typically increases.

  4. C. Miehe, S. Goektepe and J. Mendez Diez, Int. J. Of Solids and Structures, Vol. 46, 1, pages 181-202 (2009)

  5. M.D Lechner, K. Gehrke, E.H. Nordmeier, Makromolekulare Chemie, 1993

 

  • Summary

    Mechanical Properties of Plastics

    The mechanical behavior of a plastics depend on the composition, strain rate, molecular weight, crosslink density, and temperature.

  • Brittle materials break at the stress maximum and at low strain, whereas ductile materials undergo yielding followed by a drop in stress and break at noticeable lower stress but much higher strain.

  • At low stress, the deformation of most solid plastics is elastic. The applied stress is proportional to the observed strain, and after removal of the load the material returns to its original shape and size.

  • The maximum stress up to which the stress and strain remain proportional is called the proportional limit. A stress beyond the elastic limit results in permanent deformation.

  • At the yield point, the polymeric material undergoes strong irreversible plastic deformation followed by necking and, in some cases depending on strain rate and temperature.

  • Strain hardening is the increase in strength that accompanies plastic deformation beyond the yield point. It depends on the network density (physical entanglements and chemical cross-links). With increasing temperature, the strain hardening effect decreases.

  • The brittle-ductile transition temperatur is the temperature at which a polymer glass changes from brittle (crazing) to ductile (yielding) behavior in deformation and fracture.

  • The mechanical properties can be manipulated by changing the molecular weight (distribution), polymer structure, crosslink density, and polymer composition (plasticizers).

  •